| Standardization field | Metallic materials |
| Technical committee | BAS/TC 4- Steel, steel products, non-ferrous metals and alloys |
| Term (EN) | effective case depth after carburizing |
| Definition (EN) | Distance between the surface of a ferrous product and the position where the Vickers hardness is HV1 = 550 (see EU 105-71). EU 105 indicates equally that:
-loads other than the conventional load may be used after prior agreemert, to measure this depth, these loads are between 4,9 and 49 N.
-the superficial Rockwell test may be similarly used, after prior agreement to define the limiting hardness value.
|
| Term (FR) | |
| Definition (FR) | |
| Term (DE) | |
| Definition (DE) | |
| Term (BS) | efektivna dubina naugljeničenog sloja |
| Definition (BS) | Rastojanje između površine proizvoda od gvožđa i čelika i položaja gdje je tvrdoća po Vikers – u HV1 = 550 (vidi EU 105-71). Eu 105 ukazuje da:
- mogu biti korištena drugačija opterećenja od konvencionalnog opterećenja nakon što se prethodno ugovore; za mjerenje ove dubine,ova opterećenja su između 4,9 i 49 N.
- ispitivanje tvrdoće površinskog sloja metodom Rokvela može biti slično korištena, nakon što se ugovorom prethodno definiše granična vrijednost tvrdoće.
|